| Material structure | Silica aerogel held in a flexible fibrous reinforcement, commonly glass fiber felt or a similar glass-fiber web. | Confirm the reinforcement type and whether the product contains additional facing or binder layers. |
| Thermal conductivity | About 0.013–0.020 W/(m·K) is a commonly reported range for aerogel blanket products. | Compare values measured at the same mean temperature and using a stated test method; conductivity generally changes with temperature. |
| Thickness | Several thicknesses are available; 5 mm and 10 mm are common examples, with other options depending on the product. | Check actual thickness tolerance and whether the stated thickness is measured under a specified pressure. |
| Density | Varies by formulation, reinforcement, and manufacturing process; there is no single standard density for all aerogel blankets. | Request the measured density and its test method when weight or fit is important. |
| Temperature capability | The usable temperature range is product-specific and depends on the aerogel, reinforcement, facings, and operating conditions. | Use the manufacturer’s continuous and short-term temperature ratings for the complete composite, not the aerogel alone. |
| Water behavior | Some silica aerogel blankets are made to be hydrophobic; moisture resistance is not identical across all products. | Check water-repellency data and whether seams, cuts, or exposed edges need protection. |
| Handling and installation | Flexible blanket formats can be cut and fitted around many curved or irregular surfaces. | Follow the product’s installation and dust-control guidance; use suitable personal protective equipment when cutting or handling. |
| Common applications | Industrial pipes, tanks, equipment, and other locations where thin insulation or space efficiency is useful. | Confirm suitability for the operating temperature, substrate, environment, and applicable safety requirements. |
| Thermal test methods | Common methods for insulation materials include ASTM C177 and ASTM C518; the method used should be reported with the result. | Compare results only when test method, temperature, specimen conditioning, and reporting basis are clear. |